ATTENTION!!

Both the 'STANDARD' and 'PRO' models are built and operated with exactly the same magnetic process. The only thing that makes them different is their feed rate capacity per hour.  Know the amount of feed you want to process and you'll know which magnetic separator you need.

STANDARD MODEL
                               
One side of the STANDARD model features a single adjustable feed tray with its own magnetic system, and a removable black 9 inch work shelf area on the other side. A great workhorse that can run hundreds of pounds of feed per hour. See the Black Gold Magnetic Separator page for more details.

Priced well at $2795.00 (USD)(plus shipping)

FEED RATE:

Feed rate varies according to the percentage of magnetic sands in the feed stock. Testing of feeds containing 10% magnetic sands have shown the 'STANDARD' model processing over 600 lbs/hr. Average rate of feed with 100% magnetic sands is 200lbs/hr.

GOLD LOSSES FOUND IN THE SEPARATED MAGNETIC SANDS:

*Loss of gold in an enclosed water system.............................no measureable loss!
*Loss of gold larger than flour gold...........................................no measureable loss!
*Loss of flour gold...........................................................................less than a 1% loss!
*Loss of "magnetic" gold and "magnetic" platinum..............no measureable loss!

FREE TESTING:

We perform free testing on any sample sent to us (max 20lbs). We measure the percentage of "heavies" in the sample and compare it to the percentage of magnetic sands removed by the Separator. All samples need to be clean of organic material and screened through 1/8 screen.

NOTE:

A)Black Sands can vary in their magnetic strength and it is important to do
preliminary testing of your feed using the same rare-earth magnets that The Black Gold Magnetic Separator uses. They are 10 times stronger than generic ceramic magnets.
 
B) Because feed materials all vary from one place to another, we cannot guarantee specific results regarding feed rates or percentages of magnetic sands removed. Every effort was made to test a broad sampling of materials containing different kinds of gold and magnetic sands. Samples were tested from Canada, Alaska, Montana, Arizona, Colorado, Utah, North Carolina, and several sites in Oregon.  Materials came from
various sites such as placers, beach sands and hard rock mines.
C)  Unless your material is a 100% mix of strong magnetic sands and precious metals, you still need finish equipment such as a gold pan, shaker table, Spiral, Cube, etc.

Standard Model Magnetic Separator
Copyright American Gold Miner www.americangoldminer.com  All Rights Reserved.
Website Design & Hosting by RedFuel.net